HF30 A608 Centrifugal Cast Heat-Resistant Alloy

HF30 A608 Centrifugal Cast Heat-Resistant Alloy Grade:HF30 Chemical Requirements(Composition, %) C: 0.25–0.35 Mn: 1.5max Si: 0.50–2.00 Cr: 19–23 Ni: 9—12 P: 0.04 max S: 0.04 max Mo:0.50 max Minimum Elevated Temperature Tensile Strength and Elongation Values 1、1400 °F [760 °C] Tensile Strength, psi [kPa]: 26000 [180000] Elongation, %:7.0 2、1600 °F

Read More

HF A 297/A 297M (CENT, INVEST, SAND)

HF  A 297/A 297M (CENT, INVEST, SAND) Grade:HF (CENT, INVEST, SAND) Type:19 Chromium, 9 Nickel Chemical Requirements(Composition, %): Carbon:0.20–0.40 Manganese, max:2.00 Silicon, max:2.00 Phosphorus, max:0.04 Sulfur, max:0.04 Chromium Nickel:18.0–23.0 Nickel:8.0–12.0 Molybdenum, max:0.50 HF Tensile Requirements Tensile Strength, min ksi :70 [MPa]:485 Yield Point, min Ksi:35 [MPa]:240 Elongation in 2 in.

Read More

HE35 A608 Centrifugal Cast Heat-Resistant Alloy

HE35 A608 Centrifugal Cast Heat-Resistant Alloy Grade:HE35 Chemical Requirements(Composition, %) C: 0.30–0.40 Mn: 1.5max Si: 0.50–2.00 Cr: 26–30 Ni: 8—11 P: 0.04 max S: 0.04 max Mo:0.50 max Keywords:alloy; centrifugal casting; high temperatures; pressure containing parts; steel tube; temperature service applications Learn more

HE 29Chromium, 9 Nickel A297/A297M

HE Grade:HE (CENT, INVEST, SAND) Type:29 Chromium, 9 Nickel Chemical Requirements(Composition, %): Carbon:0.20–0.50 Manganese, max:2.00 Silicon, max:2.00 Phosphorus, max:0.04 Sulfur, max:0.04 Chromium Nickel:26.0–30.0 Nickel:8.0–11.0 Molybdenum, max:0.50 Tensile Requirements Tensile Strength, min ksi :85 [MPa]:585 Yield Point, min Ksi:40 [MPa]:275 Elongation in 2 in. [50 mm], min, % :9 Heat Treatment

Read More

HD50 A608 Centrifugal Cast Heat-Resistant Alloy

HD50 A608 Centrifugal Cast Heat-Resistant Alloy Grade:HD50 Chemical Requirements(Composition, %) C: 0.45–0.55 Mn: 1.5max Si: 0.50–2.00 Cr: 26–30 Ni: 4—7 P: 0.04 max S: 0.04 max Mo:0.50 max Minimum Elevated Temperature Tensile Strength and Elongation Values 1、1400 °F [760 °C] Tensile Strength, psi [kPa]: 7450 [51400] 2、1600 °F [870 °C]

Read More

HD 28 Chromium, 5 Nickel A297/A297M

Grade:HD (CENT, INVEST, SAND) Type:28 Chromium, 5 Nickel  Chemical Requirements(Composition, %): Carbon:0.5 max Manganese, max:1.50 Silicon, max:2.00 Phosphorus, max:0.04 Sulfur, max:0.04 Chromium Nickel:26.0–30.0 Nickel:4.0—7.0 Molybdenum, max:0.50 HD Tensile Requirements Tensile Strength, min ksi :75 [MPa]:515 Yield Point, min Ksi:35 [MPa]: 240 Elongation in 2 in. [50 mm], min, % :8

Read More

HC 28Chromium A297/A297M (CENT, INVEST, SAND)

HC  A297/A297M Grade:HC (CENT, INVEST, SAND) Type:28 Chromium Chemical Requirements(Composition, %): Carbon:0.5 max Manganese, max:1.00 Silicon, max:2.00 Phosphorus, max:0.04 Sulfur, max:0.04 Chromium Nickel:26.0–30.0 Nickel:4.00 max Molybdenum, max:0.50 Tensile Requirements Tensile Strength, min ksi :55 [MPa]:380  Heat Treatment Castings for heat-resistant service may be shipped in the as-cast condition without heat

Read More

H30 A608 Centrifugal Cast Heat-Resistant Alloy Tubing

H30  A 608(Centrifugal Cast Heat-Resistant Alloy Tubing) Grade:H30 Chemical Requirements(Composition, %) C: 0.25–0.35 Mn: 0.5–1.0 Si: 0.50–2.00 Cr: 26–30 Ni: 4.0 max P: 0.04 max S: 0.04 max Mo:0.50 max Minimum Elevated Temperature Tensile Strength and Elongation Values 1、1400 °F [760 °C] Tensile Strength, psi [kPa]: 5300 [36000] Elongation, %:40

Read More

CZ100 N02100 A 494/A 494M – 09

CZ100 N02100 A 494/A 494M – 09 Standard Specification for Castings, Nickel and Nickel Alloy Grade:CZ100 UNS Numbers:N02100 Alloy Family:Ni CZ100 Chemical Requirements: C(max):1.00 Mn(max):1.50 Si(max):2.00 P(max):0.03 S(max):0.03 Cu: max 1.25 Fe:max 3.00 Ni:min 95 CZ100 Mechanical  Properties Tensile strength:50min, ksi [MPa]:[345] Yield strength:18min, ksi [MPa]:[125] Elongation in 2 in:10[50 mm],A

Read More

CN7MS ASTM A743 (CENT, INVEST, SAND)

CN7MS ASTM A743 (CENT, INVEST, SAND) Grade(UNS):CN7MS (J94650) Type:19Chromium,24 Nickel,with Copper and  Molybdenum Chemical Requirements: C(max):0.07 Men(max):1.00 Si(max):2.50~3.50 P(max):0.04 S(max):0.03 Cr:18.0~22.0 Ni:22.0~25.0 Molybdenum:2.5~3.0 Copper:1.5~2.0 Heat Treatment Requirements: Heat to 2100°F [1150°C] minimum, 2150°F [1180°C] maximum, hold for sufficient time (2 h minimum) to heat casting to temperature and quench in