M35-2 Ni-Cu N24020 A 494/A 494M – 09

M35-2 Ni-Cu N24020 A 494/A 494M – 09 Standard Specification for Castings, Nickel and Nickel Alloy Grade:M35-2 UNS Numbers:N24020 Alloy Family:Ni-Cu M35-2 Ni-Cu Chemical Requirements: C(max):0.35 Mn(max):1.50 Si(max):2.00 P(max):0.03 S(max):0.03 Cu: 26.0-33.0 Fe:max 3.50 Ni:balance Cb(Nb):0.5max M35-2 Ni-Cu Mechanical  Properties Tensile strength:65min, ksi [MPa]:[450] Yield strength:30 min, ksi [MPa]:[205] Elongation

Read More

M30H Ni-Cu N24030 A 494/A 494M – 09

M30H Ni-Cu  N24030 A 494/A 494M – 09 Standard Specification for Castings, Nickel and Nickel Alloy Grade:M30H UNS Numbers:N24030 Alloy Family:Ni-Cu M30H Ni-Cu Chemical Requirements: C(max):0.30 Mn(max):1.50 Si(max):2.7-3.7 P(max):0.03 S(max):0.03 Cu: 27.0-33.0 Fe:max 3.50 Ni:balance M30H Ni-Cu Mechanical  Properties Tensile strength:100min, ksi [MPa]:[690] Yield strength:60 min, ksi [MPa]:[415] Elongation in

Read More

M30C Ni-Cu N24130 A 494/A 494M – 09

M30C Ni-Cu N24130 A 494/A 494M – 09 Standard Specification for Castings, Nickel and Nickel Alloy Grade:M30C UNS Numbers:N24130 Alloy Family:Ni-Cu M30C Ni-Cu  Chemical Requirements: C(max):0.30 Mn(max):1.50 Si(max):1.0-2.0 P(max):0.03 S(max):0.03 Cu: 26.0-33.0 Fe:max 3.50 Ni:balance Cb(Nb):1.0—3.0 M30C Ni-Cu Mechanical  Properties Tensile strength:65min, ksi [MPa]:[450] Yield strength:32.5min, ksi [MPa]:[225] Elongation in

Read More

M25S Nickel alloy castings A 494/A 494M – 09

M25S nickel alloy castings A 494/A 494M – 09 Standard Specification for Castings, Nickel and Nickel Alloy Grade:M25S UNS Numbers:N24025 Alloy Family:Ni-Cu M25S nickel alloy castings Chemical Requirements: C(max):0.25 Mn(max):1.50 Si(max):3.5-4.5 P(max):0.03 S(max):0.03 Cu: 27.0-33.0 Fe:max 3.50 Ni:balance M25S nickel alloy castings  Mechanical  Properties Hardness HB:300 HB minimum for the age

Read More

HX50 A608 Heat-Resistant Alloy Tubing

HX50 A608 Centrifugal Cast Heat-Resistant Alloy Tubing Grade:HX50 Chemical Requirements(Composition, %) C: 0.40–0.60 Mn: 1.5max Si: 0.50–2.00 Cr: 15–19 Ni:64—68 P: 0.04 max S: 0.04 max Mo:0.50 max Keywords:alloy; centrifugal casting; high temperatures; pressure containing parts; steel tube; temperature service applications Learn more

HX 17Chromium, 66 Nickel A297/A297M

HX A297/A297M Grade:HX (CENT, INVEST, SAND) Type:17 Chromium, 66 Nickel Chemical Requirements(Composition, %): Carbon:0.35–0.75 Manganese, max:2.00 Silicon, max:2.50 Phosphorus, max:0.04 Sulfur, max:0.04 Chromium Nickel:15.0–19.0 Nickel:64.0–68.0 Molybdenum, max:0.50 Tensile Requirements Tensile Strength, min ksi :60 [MPa]:415  Heat Treatment Castings for heat-resistant service may be shipped in the as-cast condition without heat

Read More

HW50 A608 Heat-Resistant Alloy Tubing

HW50 A608 Centrifugal Cast Heat-Resistant Alloy Tubing Grade:HW50 Chemical Requirements(Composition, %) C: 0.40–0.60 Mn: 1.5max Si: 0.50–2.00 Cr: 10–14 Ni:58—62 P: 0.04 max S: 0.04 max Mo:0.50 max Keywords:HW50;alloy; centrifugal casting; high temperatures; pressure containing parts; steel tube; temperature service applications Learn more

HW 12Chromium, 60 Nickel A297/A297M

HW A297/A297M Grade:HW (CENT, INVEST, SAND) Type:12 Chromium, 60 Nickel Chemical Requirements(Composition, %): Carbon:0.35–0.75 Manganese, max:2.00 Silicon, max:2.50 Phosphorus, max:0.04 Sulfur, max:0.04 Chromium Nickel:10.0–14.0 Nickel:58.0–62.0 Molybdenum, max:0.50 Tensile Requirements Tensile Strength, min ksi :60 [MPa]:415 Elongation in 2 in. [50 mm], min, % : Heat Treatment Castings for heat-resistant service may

Read More

HU50 A608 Heat-Resistant Alloy Tubing

HU50 A608 Centrifugal Cast Heat-Resistant Alloy Tubing Grade:HU50 Chemical Requirements(Composition, %) C: 0.40–0.60 Mn: 1.5max Si: 0.50–2.00 Cr: 17–21 Ni: 37—41 P: 0.04 max S: 0.04 max Mo:0.50 max Keywords:alloy; centrifugal casting; high temperatures; pressure containing parts; steel tube; temperature service applications Learn more

HU 19Chromium, 39 Nickel A297/A297M

HU A297/A297M Grade:HU (CENT, INVEST, SAND) Type:19 Chromium, 39 Nickel Chemical Requirements(Composition, %): Carbon:0.35–0.75 Manganese, max:2.00 Silicon, max:2.50 Phosphorus, max:0.04 Sulfur, max:0.04 Chromium Nickel:17.0–21.0 Nickel:37.0–41.0 Molybdenum, max:0.50 Tensile Requirements Tensile Strength, min ksi :65 [MPa]:450 Elongation in 2 in. [50 mm], min, % :4 Heat Treatment Castings for heat-resistant service may

Read More