Chemical  RequirementsComposition% Max Except as Indicated

Major Elements

Copper:86.0~89.0

Tin:9.0~11.0

Lead:0.30

Zinc: 1.0~3.0

Iron: 0.20

Nickelincl.Cobalt: 1.0

Antimony: 0.20

Residual Elements

Sulfur: 0.05

Phosphorus: 0.05

Aluminum: 0.005

Silicon: 0.005

Mechanical Requirements

Tensile Strength,min

ksi: 40

MPa: 276

Yield Strength,ᴬ min

ksi: 18

MPa: 124

Elongation in 2 in.or 50 mm, min, %: 20

Keywords

copper alloy castings; copper-base alloy castings; sand castings

Learn more

Share:

More Posts

parts of Centrifuge and dewatering equipment

CD4MCuN:Everything you should know

CD4MCuN alloy is nominally a 26Cr-6Ni alloy (C≤0.04) with the addition of molybdenum and copper. There is no corresponding deformed steel grade for this alloy.

Composite rollers of centrifugal casting

Production of High Chromium Cast Iron-Cast Steel Bimetallic Cylinder Liners Using Composite Rollers Centrifugal Casting Process High-chromium cast iron-cast steel bimetallic cylinder liners are produced

Send Us A Message