CF16Fa
Cast ASTM: A743, CF16Fa (CENT, INVEST, SAND)
Type:19 Chromium, 9 Nickel,Free Machining
Chemical Requirements:
C(max):0.16
Men(max):1.5

Si(max):2.00
P(max):0.04
S(max):0.20~0.40
Cr:18.0~21.0
Ni:9.0~12.0
Moiybdenum:0.40~0.80
Austenitic stainless steel
Heat Treatment Requirements:
Heat to 1900°F [1040°C] minimum, hold for sufficient time to heat casting to temperature, quench in water or rapid cool by other means
Tensile Requirements:
Tensile Strength, min
Tensile, ksi: 70
Tensile, MPa:485
Yield Strength, min
Yield, ksi:30
Yield, MPa:205
Elongation in 2 in. [50 mm] min, %A: 25
Keywords: corrosion resistant; iron-chromium; iron-chromium nickel; steel castings