CF3MN ASTM A743 (CENT, INVEST, SAND)
Type:19Chromium, 10 Nickel,with Molybdenum,and Nitrogen
CF3MN Chemical Requirements:
C(max):0.03
Men(max):1.50
Si(max):1.50
P(max):0.04
S(max):0.04
Cr:17.0~22.0
Ni:9.0~13.0
Molybdenum:2.0~3.0
Nitrogen:0.10~0.20
Heat Treatment Requirements:
(1) Heat to 1900°F [1040°C] minimum, hold for sufficient time to heat casting to temperature, and cool rapidly.
(2)As cast if corrosion resistance is acceptable
Tensile Requirements:
Tensile Strength, min
Tensile, ksi: 75
Tensile, MPa:515
Yield Strength, min
Yield, ksi:37
Yield, MPa:255
Elongation in 2 in. [50 mm] min, %A: 35
Keywords: corrosion resistant; iron-chromium; iron-chromium nickel; steel castings