HI35 A608 Centrifugal Cast Heat-Resistant Alloy Tubing
Grade:HI35
Chemical Requirements(Composition, %)
C: 0.30–0.40
Mn: 1.5max
Si: 0.50–2.00
Cr: 26–30
Ni: 14—18
P: 0.04 max
S: 0.04 max
Mo:0.50 max
Minimum Elevated Temperature Tensile Strength and Elongation Values
1、1600 °F [870 °C]
Tensile Strength, psi [kPa]: 20000
[138000]
Elongation, %:8.0
2、1800 °F [980 °C]
Tensile Strength, psi [kPa]: 8200
[56000]
Elongation, %:12.0
Keywords:alloy; centrifugal casting; high temperatures; pressure containing parts; steel tube; temperature service applications