HL30 A608 Centrifugal Cast Heat-Resistant Alloy Tubing

GradeHL30

Chemical Requirements(Composition, %)

C: 0.25–0.35

Mn: 1.5max

Si: 0.50–2.00

Cr: 28–32

Ni: 18—22

P: 0.04 max

S: 0.04 max

Mo0.50 max

Keywordsalloy; centrifugal casting; high temperatures; pressure containing parts; steel tube; temperature service applications