CF20 (SCS12, J92602) Cast Stainless Steel

CF20 ASTM A743&A743M(cent,invent,sand) Grade(UNS):CF20(J92602) Type:19 Chromium, 9 Nickel CF20 Chemical Requirements: C(max):0.20 Men(max):1.5 Si(max):2.00 P(max):0.04 S(max):0.04 Cr:18.0~21.0 Ni:8.0~11.0 Heat Treatment Requirements: Heat to 1900°F [1040°C] minimum, hold for sufficient time to heat casting to temperature, quench in water or rapid cool by other means metallographic structure: Austenitic stainless steel Tensile Requirements: Tensile Strength, min Tensile, ksi: 70 […]

CF8 ASTM A743/A743M

CF8 ASTM A743/A743M  (CENT, INVEST, SAND) Grade(UNS):CF8(J92600) Type:19 Chromium, 9 Nickel  CF8 Chemical Requirements: C(max):0.08 Men(max):1.5 Si(max):2.00 P(max):0.04 S(max):0.04 Cr:18.0~21.0 Ni:8.0~11.0 Heat Treatment Requirements: Heat to 1900°F [1040°C] minimum, hold for sufficient time to heat casting to temperature, quench in water or rapid cool by other means Tensile Requirements: Tensile Strength, min Tensile, ksi: 70 Tensile, […]